Methods For Improving Hardness And Strength Of Ceramic Materials
Author: Thomas, D. A. et al
Source: US Patent 3,573,023
Doc ID: 1971002
Year of Publication: 1971
Abstract:
Methods for improving the hardness and strength of frangible or relatively brittle materials, involving surface deformation by mechanical means to establish compressive stresses in the material surface.