Glass Bead Forming Method
Author: J.J. Hammel; E.J. Cone
Source: US Patent 4,002,446
Doc ID: 1977067
Year of Publication: 1977
Abstract:
Spherical regularity of glass beads is improved by catching a falling stream of hot beads in a bath of liquid quenching medium having a relatively low heat transfer coefficient controlled by maintaining a relatively high viscosity.
| Download PDF |
|---|