Process For Measuring The Level Of Metal In Vessels, Especially In Continuous Casting Molds
Author: Block, Franz-Rudolf
Source: US Patent 4,279,149
Doc ID: 1981054
Year of Publication: 1981
Abstract:
A method of measuring the level of molten metal in a continuous casting mold comprises inducing in the molten metal a magnetic field by a primary electrically energized coil and, by the relationship of this magnetic field to a pair of symmetrical secondary coils coaxial with the primary coil, inducing voltages in these secondary coils which are electrically connected in a circuit opposition so that the resultant voltage represents the level of the molten metal.