Shot Quality and How To Select Shot For Peening
Author: David Hale, Ervin Industries, Inc., Amasteel Divis
Source: The Shot Peener magazine, Vol 02/No 2, July 1988
Doc ID: 1988100
Year of Publication: 1988
Abstract:
This discussion of shot must first be preceded by a brief discussion of the basics of shot peening in order to lay the groundwork for shot selection.