Residual Stress Analysis . . .
Author: Shot Peening Staff
Source: The Shot Peener magazine, Vol 2 / No 2, July 1988
Doc ID: 1988105
Year of Publication: 1988
Abstract:
Providing Insight Into Component Failures
Residual stress exists in the majority of metallic and ceramic components. Knowing the amount, type and location of stress present in a component is important in improving the quality and reliability of the part.