U.S. Government Revises Shot Peening Specification
Author:
Source: The Shot Peener magazine, Vol 03/Issue 2, Summer 1989
Doc ID: 1989070
Year of Publication: 1989
Abstract:
U.S. Government Specification MIL-S-13165 "Shot Peening Metal Parts" has been revised to Version C. This culminates three-year project by the U.S. Army Laboratory Command, Materials Testing Laboratory, the custodian of this document. Revision B had been in effect since December, 1966.