Blast Cleaning Process Improvements
Author: Jack M. Champaigne, Electronics Inc.
Source: The Shot Peener magazine, Vol 03/Issue 2, Summer 1989
Doc ID: 1989072
Year of Publication: 1989
Abstract:
Borrowing technology from the shot peening industry, the blast cleaning of parts (casting, forgings, etc.) is deriving benefits from the Almen test strip. Historically, the cleaning process has differed from "If it's not broke, don't fix it!" type of attitude. Quality Control consisted of subjective observation of the appearance of cleaned parts.