Mathematic Model For Arc Height Saturation
Author: Shot Peening Staff
Source: The Shot Peener magazine, Vol 4 / Issue 3, Fall 1990
Doc ID: 1990155
Year of Publication: 1990
Abstract:
Measuring two Almen strips, where the exposure time for the second strip is double the first, an approximation of Almen saturation may be calculated.