The Case of the Elusive Intensity
Author: Bob Gillespie, Premier Shot Company, Inc.
Source: The Shot Peener magazine, Vol 05/Issue 2, Summer 1991
Doc ID: 1991117
Year of Publication: 1991
Abstract:
In a recent issue of "The Shot Peener", Jack Champaigne proposed that readers perform a simple test with Almen strips that involved plotting a saturation curve (qualification process), repeating this curve a number of times, peening a number of Almen strips at the saturation point, peening the same number at double the saturation time and comparing the results.