Process for Forming a Bearing Surface for Aluminum Alloy
Author: Amarjit Brar, Anthony Dierich, Prativadi Narayan
Source: US Patent 5,240,590
Doc ID: 1992068
Year of Publication: 1992
Abstract:
A process for forming a bearing surface on an aluminium alloy article including the steps peening the surface, anodizing the surface , and washing the anodized surface with a boehmite inhibiting agent.