Almen Strip as Process Control for Shot Peening
Author: Jack Champaigne, Electronics Incorporated
Source: The Shot Peener magazine, Vol 06/Issue 1, Spring 1992
Doc ID: 1992076
Year of Publication: 1992
Abstract:
Increased attention to process control for quality manufacturing in the 1990's will be necessary. How do we provide a quality program for shotpeening? This article will discuss the use, and the abuse, of the Almen strip.