Definition of Blast Pressure in Air-Operated Peening Machines
Author: R.G. Bosshard, T.T. Fritchman
Source: The Shot Peener magazine, Vol 06/Issue 3, Fall 1992
Doc ID: 1992080
Year of Publication: 1992
Abstract:
Abstract: Driving air pressure is an important parameter in air operated peening machines. Test measurements between several points in the flow system, under known loads, show the importance of establishing a clear engineering definition and specification for both system performance and air consumption.