Measurment of Shot Peening Coverage by Impact Dent Characterization
Author: Robert Thompson, Mark Tascillo
Source: US Patent 5,293,320
Doc ID: 1993018
Year of Publication: 1993
Abstract:
This invention relates to measuring shot peening coverage by impact dent characterization. Such methods of this type employ a non-distructive, automated computer analysis by analyzing dent characteristics to determine shot coverage of a particular surface.