Sensor for Lance-Type Shot Peening Guns
Author: Thompson, Robert A.
Source: US Patent 5,271,282
Doc ID: 1993020
Year of Publication: 1993
Abstract:
This invention relates to sensors of the type that are used in lance-type shot peening guns. Such structures of this type generally measure the reaction force of the ejected shot and air stream which are emitted from the lance-type shot peening gun. The sensor further supplies diagnostic information indicative of the shot peening process performance.