Residual Stress and Retained Austenite Analysis Using Windows Software
Author: New Product Release
Source: The Shot Peener magazine, Vol 7 / Issue 2, Summer 1993
Doc ID: 1993138
Year of Publication: 1993
Abstract:
TEC's X-Ray Diffraction Residual Stress and Retained Austenite Analyzer now comes with a 486DX50 personal computer (PC), Super VGA monitor and software operating under Microsoft Windows 3.1.
| Download PDF |
|---|