Standard Test Methods for Determination of Carbon, Sulfur, Nitrogen, and Oxygen in Steel and in Iron, Nickel, & Cobalt Alloys

Author:  ASTM
Source:  ASTM E 1019 - 94
Doc ID:  1994040
Year of Publication:  1994
Abstract:  
1.1 These test methods cover the determination of carbon, sulfur, nitrogen, and oxygen, in steel and in iron, nickel, and cobalt alloys having chemical compositions within the following limits:


Available from ASTM