Theoretical Basis of Shot Peening Coverage Control
Author: D. Kirk and M. Y. Abyaneh
Source: The Shot Peener magazine, Vol 09/Issue 2, Spring 1995
Doc ID: 1995057
Year of Publication: 1995
Abstract:
Abstract
A simplified treatment of the theoretical basis of coverage control is presented based on the application of an Avrami equation. This application shows how coverage progresses during shot peening with a necessary exponential approach to 100%. The effects of varying the common shot peening parameters - shot size, peening rate and exposure time are analyzed.