Research on residual stress reduction by a low frequency alternating magnetic field
Author: F. Tang, A.L. Lu, J.F. Mei, H.Z. Fang, X.J. Luo
Source: Journal of Materials Processing Technology 74 (1998) 255–258
Doc ID: 1996192
Year of Publication: 1996
Abstract:
Based on previous research of strong pulsed magnetic treatment, the effect of a low frequency alternating magnetic field on
welding residual stress was studied. The experimental results show that by low frequency alternating magnetic treatment, the
residual stresses in both rigid restrained specimens and welded specimens are reduced. Furthermore low frequency alternating
magnetic treatment has the feature of simple equipment and easy operation. © 1998 Elsevier Science S.A.