News Release, Image Analysis of Conditioned Cut Wire Pellets Gives Big Quality Gains for the Shot Peening Industry
Author: Mike Petrie, Taydor
Source: The Shot Peener magazine, Vol 11 / Issue 3, Fall 1997
Doc ID: 1997070
Year of Publication: 1997
Abstract:
The shot peening process relies for its efficiency on the maintenance of control of the medium in terms of particle size, hardness and density. Consistency is vital, not only in the original form, but also in the particles' resistance to rapid change in size and shape during the mediums' life cycle.