The Development of Residual Stresses at Bending Specimens Under the Influence of Setting and Stress Peening

Author:  E Muller
Source:  Conf Proc: ICSP-7 (pg 88-95)
Doc ID:  1999019
Year of Publication:  1999
Abstract:  
The development of the residual stresses at the surface at bending test specimens in the dependence of several parameters was investigated. The specimens had two different hardnesses (Rm = 1530; 2000N/mm