Influence of Temperature of Shot Peening on Fatigue Life
Author: Schilling-Praetzel, Hegemann, Gomez, Gottstein
Source: The Shot Peener magazine, Vol 13/Issue 1, Spring 1999
Doc ID: 1999078
Year of Publication: 1999
Abstract:
Reprinted with permission from ICSP-5 Proceedings
ABSTRACT
This paper addresses the influence of shot peening temperature on micro structure evolution and mechanical properties of spring steel 60SiCr7 in the temperature range between 200