Apparatus for Increasing the Surface Strength of Metal Components
Author: T Matsuyama; H Honda; K Ujihashi, T Ogawa
Source: US Patent 6,058,584
Doc ID: 2000005
Year of Publication: 2000
Abstract:
A casing has a processing chamber and a drying chamber defined therein by a partition mechanism. The processing chamber houses an impelling mechanism for impelling a mixed stream of glass beads and water toward a gear. First and second drying mechanisms are successively brought into the drying chamber by the partition mechanism. While the gear is being processed, i.e., peened, by the impelling mechanism in the processing chamber, a perviously processed gear is dried in the drying chamber. Gears can quickly and efficiently be peened, washed, and dried successively in the casing.