Gear Inspection System from American Stress Technologies, Inc.
Author: News Release
Source: The Shot Peener magazine, Vol 14 / Issue 1, Spring 2000
Doc ID: 2000028
Year of Publication: 2000
Abstract:
The Gear Inspection System is an off-line audit inspection system used to detect grinding damage and some heat-treat qualities, and to monitor the residual stress from manufacturing processes.