Mecshot Shot Blasting - Shot Peening Processing and Machines
Author: News Release
Source: The Shot Peener magazine, Vol 16 / Issue 1, Spring 2002
Doc ID: 2002094
Year of Publication: 2002
Abstract:
Jodhpur, India - Shot peening is the mechanical operation of introducing residual compressive surface stress on mechanical parts which are subjected to dynamic conditions like turbine blades, springs, etc. The compressive stress so produced increases fatigue life and stress corrosion resistance properties of shot peened parts. The process of shot peening is accomplished by propelling spherical shots on such parts with controlled parameters.
| Download PDF |
|---|