USF Vacu-Blast - Pass-through option now available on all USF Vacu-Blast Ventus machines
Author: News Releases
Source: The Shot Peener magazine, Vol 16 / Issue 1, Spring 2002
Doc ID: 2002095
Year of Publication: 2002
Abstract:
United Kingdom - Pictured is a USF Vacu-Blast Ventus II150P abrasive blasting cabinet machine, equipped with access doors on both sides of the blast enclosure to facilitate the "pass-through" processing of parts.