The Problem:
A manufacturer and remanufacturer of steam turbines needed to peen the root section of "bucket" blades. The blades are similar to those used in jet engines and impellers but with exceptionally large root sections - some so large, in fact, they would not fit through the vestibule of ZERO's BNP-A200/A205. (The versailte A200 and A205 can be found in just about every shop that peens turbine blades to spec, so setting one up to handle these buckets would have been a cinch.)