USF Vacu-Blast International - Universal Shot Peening Machine Developed by USF VACU-Blast for Aeroengine Components
Author: News Releases
Source: The Shot Peener magazine, Vol 16 / Issue 2, Summer 2002
Doc ID: 2002102
Year of Publication: 2002
Abstract:
United Kingdom. USF Vacu-Blast International, part of the USF Surface Preparation Group, has developed a self-contained, "universal" shot peening machine, capable of processing an extensive range of fan blades, discs and shafts from most aeroengines in current service in both the civil and defence aviation sectors. The machine improves the fatigue resistance of these critical parts, in line with aeroengine manufacturers' specifications, and can be used for both production and repair/overhaul applications.