Surface Dynamics Ltd. - New Metal Treatments Capability for Aerospace Manufacturer
Author: Industry News
Source: The Shot Peener magazine, Vol 17 / Issue 3, Summer 2003
Doc ID: 2003027
Year of Publication: 2003
Abstract:
United Kingdom. When aerospace component supplier Harmon Manufacturing decided to expand their capabilities into surface treatments, they selected Surface Dynamics Ltd. of Cheltenham to supply automated shot peening equipment. The equipment compliments Harmon's first class production, NDT and plating facilites.
| Download PDF |
|---|