Abstract:
A new laboratory, dedicated to research into the shot peening of automotive gears and transmission systems, has been opened recently at the Gear Technology Centre, operated by the Design Unit of the School of Mechanical and Systems Engineering at the University of Newcastle upon
Tyne in the north east of England.