Cast Steel Shot and Grit
Author: Ervin Industries
Source: The Shot Peener magazine, Vol 16 / Issue 4, Winter 2003
Doc ID: 2003045
Year of Publication: 2003
Abstract:
The Miracle Workers of Blast Cleaning, Profiling, Peening
Part 5 of 5 part series
Technical Bulletin June, 1996 - Reprinted with permission from Ervin Industries
In the previous chapters of this series, we have discussed how the #1 priority, QUALITY OF PRODUCT FINISH (contaminant removal and anchor-pattern profile), is affected by the user's choice of these four cast steel abrasive characteristics:
- SHAPE (Shot? Grit?);
- HARDNESS (four basic ranges);
- SIZE (as it relates to mass, or impact-power);
- SIZE (as it relates to coverage, or particle-population in the blast-stream).