RotoMate increases your blasting production!
Author: Industry News
Source: The Shot Peener magazine, Vol 18 / Issue 4, Fall 2004
Doc ID: 2004012
Year of Publication: 2004
Abstract:
The RotoMate is a unique nozzle manipulator which creates a big circular blast pattern. Driven by a pneumatic motor the nozzle makes a rotating movement and creates a blast pattern of up to 20 inches (500 mm) diameter.
| Download PDF |
|---|