Abstract:
Congratulations to Paul Prevey and Dr. Niku-Lari. Our 2003 Shot Peeners of the Year have made significant contributions to advancements in shot peening technology in industrial and academic forums. They both have demonstrated dedication and discipline that has resulted in advancing the understanding and practice of shot peening in myriad ways. We are grateful for the efforts of these pioneers whose contributions continue to improve our understanding of the peening process.