Industry News - Skew Roll Machines Provide Western Coating with Needed Profile for Rebar
Author: Shot Peening Staff
Source: The Shot Peener magazine, Vol 19 / Issue 4, Fall 2005
Doc ID: 2005083
Year of Publication: 2005
Abstract:
Burlington, Ontario. Western Coating, with plants in Eugene, Ore.; Auburn, Wash. and Ogden, Utah, is an industry leader providing epoxy-coated rebar for projects ranging from private residences to salt water piers to miles of ramps and bridges. Because coated rebar is less likely to cause concrete spalling and fracturing, it is often specified for the construction of longer-lasting structures.