Author: Shot Peening Staff
Source: The Shot Peener magazine, Volume 21 / Issue 3, Summer 2007
Doc ID: 2007016
Year of Publication: 2007
Abstract:
A successful titanium metal powder process would provide components with the same strength and weight advantages has products made from large, solid pieces of titanium, at a fraction of their present cost. Currently, few industries can justify titanium's high price tag. The opportunities are tremendous for companies that can bring a viable titanium metal powder process to market.