Flapping My Lips on the importance of a controlled shot peening process
Author: Daryll McKinley, Consulting Engineer
Source: The Shot Peener magazine, Volume 21 / Issue 3, Summer 2007
Doc ID: 2007019
Year of Publication: 2007
Abstract:
I was recently asked to review / develop a rotary flap peening certification program by a company in the aerospace industry. For the purpose of this article, I'll call them Company X. This company performs repair work on critical components, very few of which are shot peened by the original equipment manufacturer. The repair areas consist of slight damage that has been blended out and the areas are less than one square inch. Their need for shot peening is not vast, and the relatively small repair areas on the parts are well-suited to rotary flap peening.
| Download PDF |
|---|