Modern Shot Blast Solutions for the Automobile Industry
Author: Rosler Metal Finishing USA
Source: The Shot Peener magazine, Vol 21 / Issue 4, Fall 2007
Doc ID: 2007029
Year of Publication: 2007
Abstract:
New concept for adapting manufacturing processes to a changing market environment
Two of the most important issues currently facing the automotive industry are:
- Reduction of vehicle weight for better gas mileage
- Shortening the times required to bring new vehicles to the market