Author: Dr. David Kirk, Coventry University
Source: The Shot Peener magazine, Vol 23 / Issue 4, Fall 2009
Doc ID: 2009036
Year of Publication: 2009
Abstract:
INTRODUCTION
Almen arc height is the deflection of the center of an Almen strip. This deflection, when caused by bombarding one face of the strip with high
velocity shot particles, is used as a measure of the