Abstract:  
Issued 1911-06 Revised 2009-12 Superseding J403 NOV2001 RATIONALE a. Table 1 - Based on the grade survey added grades 1002, 1003, 1004, and 1007. Revised footnote 1 in table and added footnotes 2, 4 and 5. b. Table 2 - Based on the grade survey added grades 1515 and 1521. Added Residual Element footnote to table and revised notes so they don't reference Table 1. c.Table 3A - Based on the grade survey added grade 11 V41. Added Residual Element footnote to table and revised notes so they don't reference Table 1. d. Table 3B - Added Residual Element footnote to table and revised notes so they don't reference Table 1. e. Table 6 - Added additional elements to be reported for Tables 1, 3A and 3B. Deleted reference to Tables 4 and 5 since these tables are not applicable to this section. Added footnote 3. f. Tables 4 and 5 - Revised standard chemical ranges and limits, % lowest max.


This article is not for distribution
For more information:
http://www.sae.org