Shot Peening Research Keeps Pace with New Materials
Author: Kathy Levy
Source: The Shot Peener magazine, Vol 25 / Issue 3, Fall 2011
Doc ID: 2011124
Year of Publication: 2011
Abstract:
Advancements in Shot Peening by Kathy Levy
Shot Peening and its related processes are keeping pace with advancements in materials as evidenced by the quality of work presented at the Eleventh International Conference on Shot Peening
I admit that most of the material presented at ICSP-11 was over my head. I enjoy reading a paper