Almen Strip Saturation Curve needs Review
Author: Michele Bandini (Peen Service)
Source: The Shot Peener magazine, Vol 26 / Issue 2, Spring 2012
Doc ID: 2012013
Year of Publication: 2012
Abstract:
VERY DIFFERENT VALUES can be obtained when measurements or experiments are repeated. Sometimes the single values are very close to each other, other times they are far apart. Let’s have a look at two batches of numbers. They could refer, for example, to experimental measurements of the same process at different times under different settings.
| Download PDF |
|---|