Exploring Special Applications
Author: Jack Champaigne, Electronics Inc.
Source: The Shot Peener magazine, Vol 28, Issue 3, Summer 2014
Doc ID: 2014021
Year of Publication: 2014
Abstract:
The Shot Peener is covering an important resource in the shot peener’s toolbox: water. The unique benefits of water are put to good use in Cavitation Peening, Water-Jet Peening and Water-Jet Shot Peening. Two experts in these fields are sharing their knowledge with us in The Shot Peener. We’re also covering Automated Peen Forming and many more topics of value.