NanoSteel Introduces EverShotâ„¢
Author: The NanoSteel Company
Source: The Shot Peener magazine, Vol 28, Issue 3, Summer 2014
Doc ID: 2014028
Year of Publication: 2014
Abstract:
The NanoSteel® Company, a leader in nanostructured steel materials design, today announced the introduction of its proprietary EverShot™ ferrous micro peening alloy. The new material combines high hardness with a low breakage rate which allows the shot peening of parts to precision specifications. The exceptional durability of the EverShot™ peening media dramatically increases operational efficiencies leading to higher throughput and lower processing costs.