You Asked, We Answered
Author: The Shot Peener Magazine Staff
Source: The Shot Peener magazine, Vol 29, Issue 2, Spring 2015
Doc ID: 2015017
Year of Publication: 2015
Abstract:
We receive many emails requesting advice on shot peening processes and we try to answer as many as we can. By far, most of the questions pertain to the confusion between saturation, coverage and intensity so we’ve included a very good explanation by Dr. David Kirk. We’ve simplified the questions so that they do not reflect upon one particular company in respect for requests for confidentiality. These topics are a compilation of the questions we get on the same subjects.