Abstract:
The most difficult shot peening question to answer is, probably, “What peening intensity should I apply to my component?†For any specific component, an answer should be based on a combination of prior knowledge and an understanding of
the basic principles that are involved. Five basic principles are discussed as illustrated in fig.1. Prior knowledge is being aware of peening intensities that have previously been applied to similar components.