Articles of Particular Interest
Author: Jack Champaigne, Editor
Source: The Shot Peener magazine, Vol 29, Issue 4, Fall 2015
Doc ID: 2015038
Year of Publication: 2015
Abstract:
Dr. Kirk’s “Verification of Peening Intensityâ€
Peening machine parameters are established by experimental settings of machine variables and submitting Almen test strips to the blast stream for increasingly longer exposure times and graphical analysis of the arc heights. Using the 10% rule (developed by SAE in 1984), the machine peening intensity could be declared. Once the machine is placed into production, a procedure is needed to verify
its consistency.