Verification of Peening Intensity
Author: Prof. Dr. David Kirk, Coventry University, U.K.
Source: The Shot Peener magazine, Vol 29, Issue 4, Fall 2015
Doc ID: 2015045
Year of Publication: 2015
Abstract:
Verification of peening intensity is described in SAE J443 using just the three paragraphs of section 3.5. This article attempts to provide a much fuller explanation of the basic issues involved when attempting verification. These issues are summarized in fig.1. In tackling these issues we have first
to consider just what (or which) defined peening intensity has to be verified. Different problems arise depending on if a single strip holder is being used or if multiple holders are involved. For the latter case, SAE J443 introduces the concept of a “Target Arc Heightâ€.