Hydro Honing Labs Receives Patent on 3D Modeling Process
Author: Peening Technologies
Source: The Shot Peener magazine, Vol 30, Issue 1, Winter 2016
Doc ID: 2016006
Year of Publication: 2016
Abstract:
Hydro Honing Laboratories , the parent company of Peening
Technologies, has patented a process for producing Almen strip fixtures utilizing 3D modeling called “Apparatus and Method for Quantifying Metal Surface Treatmentâ€
(Patent Number US 9,063,049 B2). The process was developed by Thomas Beach and
Walter Beach of Peening Technologies and is already in use at Peening Technologies’two shot peening job shops in Connecticut and Georgia.