A New Study: “Shot Blasting and Sand Blasting in Sub-Saharan Africaâ€
Author: The Shot Peener Staff
Source: The Shot Peener magazine, Vol 30, Issue 1, Winter 2016
Doc ID: 2016012
Year of Publication: 2016
Abstract:
Sub-Saharan Africa enjoys the highest growth rate in the world. A group of countries (Nigeria, Gabon, Angola, Ghana,Ivory Coast, Cameroon, and Kenya) are on the same path as Southeast Asia in the 80s. Their growth will unfold even faster,
driven by lavish Oil and Gas production and considerable mining operations. Less known are 40 vehicle assembly plants in 10 of these countries, 30+ foundries and forges, a dozen of significant shipyards, gas bottle reconditioning, corrosion
protection and structural steel processing.