Making a Contribution to the Future
Author: Jack Champaigne, Editor
Source: The Shot Peener magazine, Vol 32, Issue 3, Summer 2018
Doc ID: 2018029
Year of Publication: 2018
Abstract:
I came across some notes from earlier SAE
meetings that included projects on coverage and
intensity determination. Numerous meetings were
dedicated to these projects. Here we are nearly 35 years
later and we’re still talking about the same subjects at
our meetings.
Does this mean we just cannot get it right or is the
technology evolving? I think it is the latter. Technology
is evolving rapidly. Now, in addition to quality
improvements in the Almen strip performance, we
are seeing progress with non-destructive testing
during high-volume production. Our SAE committee
recently established a task group to explore the use of
image analysis for media size and shape inspection
which could go a long way in removing subjective inspection results and reduce the inspection time. It seems like the only thing that remains constant is that everything
is changing.