Vibratory Peening: Promising Performance
Author: Kumar Balan
Source: The Shot Peener magazine, Vol 33, Issue 3, Summer 2019
Doc ID: 2019027
Year of Publication: 2019
Abstract:
In the Winter 2018 issue of The Shot Peener, we
discussed two non-conventional peening techniques—one of
which was Vibratory Peening. In addition to the superior surface
finish, we learnt that the layer of compression was deeper with
vibratory peening when compared to conventional shot peening.
The process itself was significantly different from conventional
peening in terms of media life, dust generation and utility
costs. We concluded that this technique of generating residual
compressive stress was worth further exploration. The results are
discussed here.